K-System II

Description

The K-System II utilizes a line-source probe to measure thermal conductivity. Thermal conductivity is a measure of the rate of heat conduction of the material and is used in heat transfer calculations. The line-source method measures thermal conductivity in both melt and solid state.

Operating Range

Temperature: 30°C to 340°C
Range: 0.1 to 4 W/m.K

Application

melt and solid state thermal conductivity
Our K-System II used in material testing